[email protected] WhatsApp +86 159 0085 2030 Qingpu, Shanghai Reply within 1 business day

Grade guides: one technical page per alloy

For each grade we publish a full technical page: nominal composition, mechanical and physical properties, corrosion behaviour, applications by industry, the standards each product form follows, and fabrication notes. New guides are added regularly — two grades at a time — until the whole range we supply is covered.

Inconel 617 UNS N06617 · W.Nr 2.4663 The cobalt-bearing creep alloy: 10–15 % Co in solid solution keeps 617 load-bearing to 950 °C, with 10,000-hour rupture strength of 170 MPa at 650 °C falling to 30 MPa at 900 °C — why 625 runs out of strength above 700 °C, the aluminium-backed scale that survives cycling to 980 °C, the nitriding weakness that sends you to Haynes 230, and welding with ERNiCrCoMo-1 and no PWHT 22 Nov 2026 Haynes 230 UNS N06230 · W.Nr 2.4733 Fourteen percent tungsten instead of cobalt: 98 MPa of 10,000-hour rupture strength at 760 °C on a yield plateau of 275 MPa that runs from 540 to 760 °C, oxidation to 1,150 °C, the best nitriding resistance of any wrought nickel alloy, no sigma or mu phase after 16,000 hours at 649–871 °C, and the Haynes thickness comparison that makes a 230 part roughly a quarter the wall of Hastelloy X 22 Nov 2026 Hastelloy X UNS N06002 · W.Nr 2.4665 The gas-turbine combustor standard: oxidation resistance to 1,200 °C, hot strength to 980 °C — and why it is not a wet-acid alloy. 21 Nov 2026 Zirconium 702 UNS R60702 · CP zirconium Commercially pure zirconium for HCl, acetic acid and urea duty: the reducing-acid mirror image of titanium, with the ASTM numbers and hydrogen-embrittlement traps. 21 Nov 2026 Titanium Gr.2 UNS R50400 · W.Nr 3.7035 The workhorse commercially pure titanium: 99.2 % Ti with oxygen as the only 'alloying' element, ASTM minimums of 345/275 MPa with typical 345–500 MPa tensile at 4.51 g/cm³ density, why it is essentially immune to ambient seawater, wet chlorine and nitric acid — and the three hard limits (HF, hot reducing acids, dry chlorine) plus the hydrogen-pickup and weld-contamination traps that decide real-world service 20 Nov 2026 Titanium Gr.5 (Ti-6Al-4V) UNS R56400 · W.Nr 3.7165 The alloy behind ~90 % of all titanium: alpha-beta 6 % Al + 4 % V giving 895–1,100 MPa at 4.43 g/cm³, the condition table that matters (annealed B348 828/895 vs plate B265 880/950 vs STA), the ~400 °C service ceiling and the 290–430 °C hot-salt SCC trap, why thermal conductivity of 6.7 W/m·K drives machining cost, and the PO discipline — condition, product standard, ELI chemistry — that prevents a misquoted Grade 5 20 Nov 2026 XM-25 / Custom 450 UNS S45000 / Type XM-25 · W.Nr 1.4594 The 17-4 upgrade path: one specified point of molybdenum (0.5–1.0 %, absent in 17-4) plus niobium stabilisation gives ~1,240–1,350 MPa at H900 with better corrosion than 17-4 and no-preheat weldability — the full condition ladder A/H900 to H1150 with typical mill ranges, the ~0.1 % ageing shrink that forces finish-machining before ageing, the H1150-at-11 °C-below-Ac1 furnace trap, PREN ≈ 17–19 and the honest 304-class corrosion envelope, and the XRF Cu+Mo signature that separates it from 17-4 and 15-5 19 Nov 2026 A286 UNS S66286 / AISI 660 · W.Nr 1.4980 The iron-base superalloy that holds hot flanges together: Ni₃(Ti,Al)-aged austenitic strength of ≥895 MPa minimum (typical 930–1,050 MPa) usable from cryogenic temperature to ~650–700 °C, non-magnetic with permeability 1.007–1.010, the 16.5 ×10⁻⁶ /K expansion match to 304/316 that makes it the anchor of ASTM A453 Grade 660 bolting, why Ti content on the certificate predicts aged strength, and why it machines like a 300-series stainless while serving like a superalloy 19 Nov 2026 Custom 455 UNS S45500 / Type XM-16 The ultra-high-strength end of the PH family: a single 4-hour ageing treatment at 482–538 °C lifts yield to 1,515 MPa minimum (typical 1,689 MPa at H900) with only ~0.001 in/in distortion, the full ASTM A564 XM-16 minimum ladder from H900 to H1050 plus Carpenter-class typicals, why notch sensitivity falls as ageing temperature rises (H1000 for threaded parts), PREN ≈ 13 and the honest atmospheric-only corrosion envelope, the Ti-content certificate check that predicts aged strength, and machining-before-ageing practice for surgical and dental instruments 18 Nov 2026 17-7 PH UNS S17700 / 631 · W.Nr 1.4568 The semi-austenitic PH grade: soft, formable and non-magnetic in Condition A, then hardened by conditioning plus ageing to 1,140–1,690 MPa with minimal distortion — the TH1050 / RH950 / CH900 routes with reference heat-treatment cycles (including the −73 °C sub-zero step), the 25 % spread in published RH950 minimums and why the PO must state condition + product standard, the magnet check that verifies hardening actually happened, PREN ≈ 17 means 304-class corrosion, and the 315–425 °C over-ageing service ceiling 18 Nov 2026 15-5 PH UNS S15500 / XM-12 · W.Nr 1.4545 The forging-grade version of 17-4: why moving 1.5 points of chromium into nickel suppresses delta ferrite and buys 30–50 % better transverse ductility in heavy sections, the full ASTM A564 / AMS 5659 ladder from Condition A through H900, H1025, H1075, H1150 and H1150M, physical properties including the 0.22 % shrinkage at H1150, why PREN ≈ 15–16 means the corrosion argument is settled elsewhere, forging and solution-treatment practice (1,040 °C, quench below 32 °C within one hour), ER630 welding, aerospace and valve-body applications, and the certificate checks that separate 15-5 from 17-4 17 Nov 2026 17-4 PH UNS S17400 / 630 · W.Nr 1.4542 The workhorse of precipitation hardening: Cu 3.0–5.0 and Nb+Ta 0.15–0.45 for 1,310 MPa at H900 from a single 482 °C age, the complete ASTM A564 table from Condition A through H900, H925, H1025, H1075, H1100, H1150 and H1150M with hardness and reduction of area, physical properties and the 0.045–0.22 % ageing shrinkage, why PREN ≈ 16 makes it a 304-class alloy and not a seawater material, the 300 °C ceiling and the 400–500 °C embrittlement band, the H900-versus-H1150 SCC trade-off for sour service, applications by industry, AMS 5643 / A693 / A705 standards, machining and ER630 welding, and the Cu + Nb PMI check that exposes a 420 or 431 substitution 17 Nov 2026 Ferralium 255 UNS S32550 / F61 · W.Nr 1.4507 The copper-bearing super duplex: why 1.5–2.5 % Cu buys dilute sulphuric and phosphoric acid resistance that 2205 and 2507 do not have, ASTM A240 minima of 550 / 760 MPa and 302 HBW, physical data to 500 °C, and the PREN arithmetic that matters most — the specification minimum only computes to 35.2, so write PREN ≥ 40 on the order, plus NACE MR0175 hardness and ferrite limits, a full comparison with 2205 / 2507 / Zeron 100 / 904L / Alloy 20, ER2594 versus ER2553 welding, and the XRF copper check that exposes a 2507 substitution 16 Nov 2026 PH 13-8 Mo UNS S13800 / XM-13 · W.Nr 1.4534 The aerospace PH stainless: Al 0.90–1.35 and Mo 2.0–2.5 for 1,415 MPa at H950 with the best stress-corrosion resistance in the family, the full AMS 5629 table from H950 to H1150 (including the H1150 yield figure that sources disagree on), physical properties, why PREN ≈ 20 means marine atmosphere yes but seawater immersion no, the H950-versus-H1025 SCC trade-off, solution anneal at 927 °C with optional cryogenic treatment, aerospace / nuclear / oil and gas applications, ER630 welding and the Al + Mo PMI check that proves you were not shipped 17-4 16 Nov 2026 Super duplex 2507 UNS S32750 · W.Nr 1.4410 The reference super duplex: 25 Cr / 4 Mo / 0.27 N for PREN 40–43, why the specification minimums only compute to 37.7 (so state PREN ≥ 40), ASTM A240/A276/A790 minima with typical mill ranges, physical data to 400 °C, CPT/CCT and warm-seawater limits, the 300 °C ceiling and 600–900 °C sigma trap, applications from subsea hubs to RO trains, ER2594 welding and the G48 purchasing checks that catch a bad quench 15 Nov 2026 Zeron 100 UNS S32760 / F55 · W.Nr 1.4501 The tungsten- and copper-bearing super duplex: W 0.5–1.0 / Cu 0.5–1.0 and the PREN formula that credits 0.5 W, 550/750 MPa minima by product form with 45 J at −46 °C, physical properties, sour-service (NACE MR0175) and dilute-sulphuric margin, a full 2205 / 2507 / Zeron 100 comparison, the 'super duplex' substitution trap, ER2594 welding and PMI verification 15 Nov 2026 Duplex 2205 UNS S32205 / S31803 · W.Nr 1.4462 The default duplex: twice the yield of 316L at PREN ≈ 34–36, ASTM A240/A276/A790 minima with typical mill values, physical data, chloride-SCC behaviour and the 250–300 °C and hot-seawater limits, S32205 vs S31803 certification, applications from O&G flowlines to chemical tankers, ER2209 welding and A923 purchasing checks 14 Nov 2026 Duplex 2304 UNS S32304 · W.Nr 1.4362 The lean duplex replacing 304L/316L: no molybdenum, half the nickel, twice the yield (≥ 400 MPa) and 316L-level PREN with duplex SCC immunity, ASTM A240 minima with typical values, the ASTM vs EN composition-window spread, applications from tanks and rebar to coastal structures, ER2209 welding and when to step up to 2205 14 Nov 2026 317L UNS S31703 · W.Nr 1.4438 The 3–4 % Mo step above 316L: what the extra chromium, nickel and molybdenum actually buy, ASTM A240/A276/A312 minima with typical mill values, physical data, PREN ≈ 29–31 limits and why it is not a seawater alloy, 317L vs 316L vs 317LMN vs 904L selection table, applications from bleach plants to FGD, ER317L welding and the Mo-3.0 % substitution trap 13 Nov 2026 321 / 347 / 321H / 347H UNS S32100 / S34700 / S32109 / S34709 · W.Nr 1.4541 / 1.4550 The stabilised grades for 425–900 °C service: how titanium and niobium stop sensitisation, the stabiliser ratios that actually govern acceptance (Ti ≥ 5×C, Nb ≥ 10×C), 321 vs 347 vs the H variants by product form, oxidation and creep limits, polythionic-acid and refinery duty, applications from exhaust systems to reformer internals, ER347 welding and the purchasing checks that matter 13 Nov 2026 Alloy 20 UNS N08020 · W.Nr 2.4660 The dedicated sulfuric-acid austenitic (Carpenter 20Cb-3): what Cu, Mo and Nb actually do, ASTM B463 mechanical minima with typical mill values, physical data, the H2SO4 concentration/temperature envelope, PREN ≈ 26–31 limits, applications by industry, ER320LR welding and a purchasing checklist 12 Nov 2026 310S / 310H UNS S31008 / S31009 · W.Nr 1.4845 The 25 % Cr / 20 % Ni heat-resistant austenitic: 310S vs 310H carbon control and why PMI cannot tell them apart, oxidation limit near 1,150 °C, creep design above 600 °C, the 600–900 °C sigma-phase trap, applications from furnace retorts to kiln internals, ER310 welding and purchasing checks 12 Nov 2026 AL-6XN UNS N08367 · W.Nr 1.4478 The American 6 % Mo super-austenitic: composition and the role of N, Mo and Cu, ASTM B688 mechanical minimums with typical mill values, PREN ≈ 46 seawater pitting data, applications from desalination to FGD, plus ERNiCrMo-3 welding and purchasing rules 11 Nov 2026 Sanicro 28 UNS N08028 · W.Nr 1.4563 The sour-service and wet-phosphoric-acid specialist: 31 % Ni / 27 % Cr composition, annealed mechanical minimums and typical values, PREN ≈ 38–40, NACE MR0175 sour-gas compliance, applications from OCTG to fertiliser evaporators, plus welding and purchasing notes 11 Nov 2026 254SMO UNS S31254 · W.Nr 1.4547 The 6 % Mo super-austenitic stainless: composition and the role of Mo, N and Cu, PREN 43 pitting and crevice data with critical pitting temperatures, mechanical values by product form, applications from desalination to FGD, plus welding and purchasing rules 10 Nov 2026 904L UNS N08904 · W.Nr 1.4539 The copper-bearing super-austenitic stainless for sulphuric acid: why Cu decides the grade, PREN 35 measured against 254SMO, the 400 °C sigma limit, acid and chloride corrosion envelopes, applications by industry, welding with ER385, and the EN 1.4539 vs ASTM dual-certification trap 10 Nov 2026 Nimonic 80A UNS N07080 · W.Nr 2.4952 / 2.4631 The original gamma-prime-hardened nickel superalloy: composition, aged minima vs typical values to ASTM B637, creep data to 815 °C, the 80A vs A286 vs 90 selection rule, plus heat-treatment, welding and purchasing guidance 10 Nov 2026 Nimonic 90 UNS N07090 · W.Nr 2.4969 / 2.4632 Cobalt-strengthened Nimonic for creep duty to ~920 °C: what 15–21 % Co buys over 80A, aged mechanical values, spring-wire strengths, the 718 vs 80A vs 90 temperature ladder, plus welding-in-solution and purchasing rules 10 Nov 2026 Hastelloy B-2 UNS N10665 · W.Nr 2.4617 The hydrochloric-acid benchmark Ni-Mo alloy: composition, annealed minima vs typical values, physical data, the oxidising-contaminant rule that decides B-2 vs C-276, plus thermal-stability and welding precautions 09 Nov 2026 Nickel 200 / 201 UNS N02200 · N02201 · W.Nr 2.4060 / 2.4061 Commercial-purity nickel for caustic soda, food plant and electrical duty: composition, annealed properties, 70–80 W/m·K conductivity, the 315 °C graphitisation rule that separates 200 from 201, and fabrication notes 09 Nov 2026 Hastelloy C-276 UNS N10276 · W.Nr 2.4819 The general-purpose Ni-Cr-Mo-W workhorse: composition, ASTM minima vs typical values, PREN ≈ 69 pitting resistance, wet-chlorine and mixed-acid selection rules, plus welding and NACE sour-service notes 08 Nov 2026 Hastelloy C-22 UNS N06022 · W.Nr 2.4602 The broader-spectrum C-family alloy: higher chromium for oxidising media, nitric-HF pickling and FGD service, physical data, C-22 vs C-276 selection rules and the mandatory rapid-quench anneal 08 Nov 2026 Monel 400 UNS N04400 · W.Nr 2.4360 The nickel-copper specialist for hydrofluoric acid and flowing seawater: composition, mechanical minima by product form, physical data, reducing-media corrosion rules and welding notes 07 Nov 2026 Monel K-500 UNS N05500 · W.Nr 2.4375 The age-hardenable Monel: gamma-prime ageing cycle, properties by condition and section size, non-magnetic drill collars and pump shafts, plus the HF and hydrogen-embrittlement limits 07 Nov 2026 Incoloy 825 UNS N08825 · W.Nr 2.4858 The titanium-stabilised acid workhorse: composition, properties by product form, sulphuric and phosphoric acid selection rules, welding and buying notes 06 Nov 2026 Incoloy 925 UNS N09925 The age-hardenable 825: gamma-prime strengthening, solution-annealed vs STA properties, NACE MR0175 sour-service limits and wellhead applications 06 Nov 2026 Inconel X-750 UNS N07750 · W.Nr 2.4669 Precipitation-hardened spring and fastener grade: aged vs annealed properties, heat-treatment schedules I–III, relaxation resistance and turbine applications 05 Nov 2026 Incoloy 800 / 800H UNS N08800 / N08810 · W.Nr 1.4876 / 1.4958 Iron-base heat-resistance workhorse: 800 vs 800H vs 800HT differences, creep-rated service above 600 °C, reformer and pyrolysis applications 05 Nov 2026 Inconel 693 UNS N06693 · EN 2.4650 The metal-dusting reference grade: Ni-Cr-Al composition, properties, syngas and reformer applications, supply standards 04 Nov 2026 Inconel 690 UNS N06690 · W.Nr 2.4642 High-chromium SCC-resistant grade: annealed vs TT condition, nuclear steam-generator and caustic/nitric applications 04 Nov 2026 Inconel 600 UNS N06600 · W.Nr 2.4816 Composition, mechanical and physical properties, caustic and chloride-SCC resistance, oxidation to 1,095 °C 03 Nov 2026 Inconel 601 UNS N06601 · W.Nr 2.4851 Alumina-forming heat-resistance grade: properties, oxidation to 1,180 °C, carburisation and furnace applications 03 Nov 2026 Inconel 718 UNS N07718 · W.Nr 2.4668 Composition, heat treatment (double ageing), mechanical properties and applications 03 Nov 2026 Inconel 625 UNS N06625 · W.Nr 2.4856 Composition, properties (PREN ≈ 50), corrosion resistance, applications and welding 03 Nov 2026

Missing a grade?

Tell us which alloy you are working with — we will send the technical data and a quotation within one business day.

Ask for your grade