Inconel 690 (UNS N06690): composition, properties and applications

Inconel 690 is the high-chromium member of the Inconel family: a solid-solution Ni-Cr-Fe alloy with 27–31 % chromium, developed specifically to fix the stress-corrosion cracking problems that limited Alloy 600 in hot water and caustic service. It is the reference material for nuclear steam-generator tubing, and a cost-effective choice for nitric acid and caustic equipment where ordinary stainless steels crack. This guide pulls together the composition limits, mechanical and physical data, the annealed-vs-TT selection logic and the supply standards we use when quoting 690 bar, plate, pipe and forgings.

Machined nickel alloy forged discs

What Inconel 690 is — in one paragraph

Inconel 690 (UNS N06690, W.Nr 2.4642) is a nickel-base alloy with a nominal 60 % nickel, 29 % chromium and 9 % iron balance. It was engineered as the successor to Alloy 600: by raising the chromium content from about 15 % to 27–31 %, the grain-boundary chemistry in high-temperature water and caustic environments shifts decisively in favour of intergranular stress-corrosion resistance. The result is a solid-solution alloy that is non-age-hardenable, easy to fabricate, and today the international reference for nuclear steam-generator tubing. Outside the nuclear world, the same high-chromium metallurgy delivers excellent performance in nitric acid, polythionic acids and hot caustic, plus oxidation resistance to roughly 1,100 °C.

Nominal chemical composition

ElementContent (wt %)Why it matters
Nickel (Ni)58 minAustenitic base; chloride-SCC immunity and caustic compatibility
Chromium (Cr)27–31The defining element — stable Cr₂O₃ scale, grain-boundary Cr₂₃C₆ after TT, outstanding SCC and nitric-acid resistance
Iron (Fe)7–11Stabilises the structure, contributes solid-solution strength
Carbon (C)0.05 maxVery low to control sensitisation in the weld HAZ
Manganese (Mn)0.5 maxDeoxidation and sulfur control
Silicon (Si)0.5 maxProcessing control; supports oxidation resistance
Copper (Cu)0.5 maxResidual, kept low to preserve corrosion performance

For nuclear orders, cobalt is typically restricted as a residual (often ≤ 0.10 % or lower by agreement) to limit activation in the primary circuit — confirm the limit with the specification before ordering.

Mechanical properties

Minimum values per ASTM B166 (bar, annealed) with typical mill-certificate ranges in brackets. 690 is a solid-solution grade: the optional TT thermal treatment improves stress-corrosion resistance but does not raise strength.

ConditionYield strength (0.2 %)Tensile strengthElongation
Annealed — ASTM B166 minimum≥ 240 MPa≥ 585 MPa≥ 30 %
Annealed — typical mill values330–450 MPa670–800 MPa35–45 %
TT (thermally treated, 700–730 °C)same strength basis as annealedsame strength basis as annealed30–40 %

Design notes: yield falls gently with temperature (roughly 70 % of the room-temperature value near 500 °C). Modulus of elasticity is about 211 GPa at room temperature. Nuclear code work is always performed to the customer's written procedure, with furnace charts supplied alongside the EN 10204 3.1 certificate.

Physical properties

PropertyValue
Density8.19 g/cm³
Melting range1,343–1,377 °C
Thermal conductivity (room temp)≈ 13.5 W/m·K (rises to ≈ 23 W/m·K at 600 °C)
Specific heat≈ 450 J/kg·K
Thermal expansion (20–100 °C)≈ 14.1 ×10⁻⁶ /K
Electrical resistivity≈ 1.15 µΩ·m
Magnetic behaviourEssentially non-magnetic

Corrosion resistance — why 690 replaced 600

  • High-temperature water (nuclear primary): intergranular SCC that affected Alloy 600 in pure deoxygenated water is effectively suppressed. The optional TT treatment (a 700–730 °C hold of 10–16 h) precipitates semi-continuous chromium carbides on grain boundaries and is the specified condition for nuclear steam-generator tubing.
  • Caustic (NaOH): markedly better than 600 and far better than austenitic stainless steels up to several hundred °C — the grade of choice for caustic evaporator hardware.
  • Nitric acid: excellent, including in the hot, concentrated duties where 304L/310L begin to suffer intergranular attack — used for nitric-acid cooler condensers and reboilers.
  • Polythionic acid / sulphides: resistant where sensitised 18-8 stainless cracks; useful in refinery and sour-water environments.
  • Oxidation: forms a tight, adherent Cr₂O₃ scale — good service in static air up to about 1,100 °C.

Selection rule of thumb: if the governing failure mode is stress-corrosion cracking in hot water, caustic or nitric service, step from 600/304L up to 690. If the medium is reducing hot acid (HCl, dilute H₂SO₄), 690 is not the answer — look at Hastelloy B/C family instead. And if carburising syngas causes metal dusting, 693 is the grade designed for that.

Typical applications

IndustryTypical 690 components
Nuclear powerSteam-generator tubing (690TT), tube supports, primary-circuit internals, replacement parts for Alloy 600 components
Chemical processingNitric-acid cooler condensers, reboilers and plant piping; caustic evaporators and concentrators
RefiningPolythionic-acid service hardware, sour-water stripper internals
Heat treatmentFurnace fixtures and radiant sections needing oxidation resistance to ~1,100 °C with SCC resistance on top
Waste treatmentComponents for oxidising and alkaline waste streams

Standards and product forms we supply

  • Seamless pipe & tube: ASTM B167 / B163 (ASME SB167 / SB163)
  • Plate / sheet / strip: ASTM B168 / ASME SB168
  • Bar / rod: ASTM B166 / ASME SB166
  • Welded fittings: ASTM B366
  • German equivalents: DIN 17750–17752 (W.Nr 2.4642)
  • Nuclear practice: RCC-M M4101 procurement for French-standard nuclear work
  • Weld wire / electrodes: ERNiCrFe-7 (AWS A5.14, FM-52), ENiCrFe-7 (AWS A5.11)
  • Forged flanges, rings, blocks, machined parts: supplied to drawing with EN 10204 3.1 certificates

Welding and fabrication notes

690 welds with the same discipline as other Inconel grades: no preheat, TIG/MIG/PAW with ERNiCrFe-7 (FM-52) filler, interpass temperature kept below 150 °C and low heat input on the root pass. Do not dilute the weld with carbon-steel or stainless fillers — the high-chromium filler is what carries the corrosion performance into the joint. For nuclear and caustic duty, the welded assembly is commonly given the TT treatment (700–730 °C, 10–16 h) after welding so the HAZ gets the same grain-boundary morphology as the base metal; specify this on the purchase order, since it is an extra furnace cycle. Solution annealing (roughly 1,040–1,100 °C followed by water quench) restores ductility after heavy forming. One naming note: 690TT is not an aged or precipitation-hardened condition — no strength increase should be expected from it.

Buying 690 from Hangbo

We supply Inconel 690 bar, plate, seamless pipe, forgings and machined parts, in annealed or TT condition as your specification requires, with EN 10204 3.1 mill certificates and PMI verification before packing. Nuclear-facing orders are quoted with the customer's procurement procedure attached from the RFQ stage so that heat-treatment records and test scope match first time. Typical lead time: 15–30 days for stock and mill- stocked sizes, 45–60 days for forged or TT-treated parts produced to order.

Frequently asked questions

What is the 690TT condition?

A thermal treatment at 700–730 °C held for 10–16 hours after solution annealing. It precipitates semi-continuous chromium carbides along grain boundaries, which is the microstructure that resists intergranular SCC in nuclear primary water and hot caustic. It does not increase strength — 690 is not a precipitation-hardening alloy.

Why is 690 specified instead of Alloy 600?

600 with about 15 % Cr was prone to intergranular stress-corrosion cracking in hot deoxygenated water and caustic. Raising chromium to 27–31 % in 690 suppresses that mechanism. Most modern nuclear steam generators and 600 replacements use 690TT.

Is Inconel 690 magnetic?

No — the alloy is fully austenitic and essentially non-magnetic in all supplied conditions.

690 vs 693 — which do I need?

Both share roughly 29 % Cr. 690 is the general high-chromium corrosion/SCC grade (nuclear, nitric acid, caustic). 693 adds ~3 % aluminium and is engineered specifically for metal-dusting resistance in carburising syngas. If your failure mode is metal dusting, choose 693; for SCC in water or caustic, 690.