[email protected] WhatsApp +86 159 0085 2030 Qingpu, Shanghai Reply within 1 business day

Inconel 601 (UNS N06601): the alumina-forming heat-resistance grade

Inconel 601 is the heat-resistance specialist of the Ni-Cr-Fe family. Its 1.0–1.7 % aluminium grows a tightly adherent Al₂O₃ scale instead of the chromium oxide that 600 relies on, and that single change is why 601 holds up to about 1,180 °C and survives thermal cycling that spalls lesser alloys. This guide covers the numbers, the atmosphere limits where 601 is the right answer, and the places where 600 or 625 will do the same job for less money.

Machined nickel alloy forged discs

What Inconel 601 is — in one paragraph

Inconel 601 (UNS N06601, W.Nr 2.4851, NiCr23Fe) is a nickel-chromium-iron alloy with 58–63 % nickel, 21–25 % chromium and 1.0–1.7 % aluminium. It was developed specifically as a heat-resistance grade: the aluminium oxidises preferentially at the surface and forms a dense, slow-growing Al₂O₃ layer that stays adherent through heating and cooling cycles. The result is continuous service capability in air to about 1,180 °C — a good 80–100 °C above 600 — with markedly better resistance to spalling and to carburisation.

Chemically it is close to 600 with more chromium and the aluminium addition: 601 gives up some of 600's caustic and high-purity-water performance in exchange for high-temperature durability. It is still a solid-solution alloy with no ageing treatment, still fully austenitic, still non-magnetic, and still readily weldable — which is why it dominates furnace furniture, radiant tubes and heat-treat fixtures.

The trade-off to keep in mind: aluminium makes the alloy stronger and more oxidation resistant, but also less forgiving in the mill — narrower hot-working windows, more careful annealing to avoid grain growth, and a weld pool that is slightly less fluid than 600. None of that is a problem for a competent fabricator, but it does show up in lead time and price.

Nominal chemical composition

Composition limits per ASTM B168 / B166 / B167 (UNS N06601), weight percent:

ElementContent (wt %)Why it matters
Nickel (Ni)58.0–63.0Austenitic matrix; chloride-SCC resistance; ductility retention after long high-temperature exposure
Chromium (Cr)21.0–25.0More than 600 — higher hot corrosion and sulphidation resistance, and a stronger Cr₂O₃ base layer under the alumina
Aluminium (Al)1.0–1.7The defining addition. Forms the protective Al₂O₃ scale; also gives a modest strength increase through Ni₃Al-type precipitation on long service
Iron (Fe)Balance (nominally 13–17)Cost balance and austenite stability
Carbon (C)0.10 maxCapped lower than 600 — less grain-boundary carbide, better resistance to sensitisation on slow cooling
Manganese (Mn)1.0 maxDeoxidation
Silicon (Si)0.5 maxDeoxidation; too much silicon would embrittle the alumina scale
Copper (Cu)1.0 maxResidual limit
Sulphur (S)0.015 maxHot ductility and weld soundness

The difference between 600 and 601 in one line: 600 is a corrosion alloy that tolerates heat; 601 is a heat-resistance alloy that tolerates moderate corrosion. 1.0–1.7 % aluminium is what buys the extra 100 °C and the cycling tolerance — and what costs you 600's caustic performance.

Mechanical properties

Room-temperature tensile properties, solution-annealed condition. The ASTM minima are what a certificate must show; the typical range is what our mills actually report.

Condition0.2 % yield strengthTensile strengthElongationHardness
Annealed — ASTM B168 minimum≥ 205 MPa≥ 550 MPa≥ 30 %Not specified
Annealed — typical mill certificate300–380 MPa650–850 MPa30–40 %150–220 HB
Cold-rolled sheet, temper-rolledBy agreement, typically 450–700 MPaBy agreement, typically 750–950 MPa≥ 15–25 %Reported per heat

Note the gap. The ASTM minimum yield (205 MPa) is far below what the mills actually deliver (300–380 MPa), so a certificate showing 330 MPa is not a premium heat — it is normal. The wide gap exists because the standard also has to cover heavy plate and large forgings with coarser grain.

Elevated temperature. 601 keeps useful strength to about 900 °C, but above roughly 600 °C design must be based on creep and rupture data rather than tensile values, and above 900 °C the alloy is chosen for scale resistance, not for load-bearing. Long exposure at 600–800 °C can harden 601 slightly through aluminium-related precipitation; that is expected and is not a reason to reject a heat.

Physical properties

PropertyValueComment
Density8.11 g/cm³Lighter than 600 (8.47) — worth knowing on large furnace fixtures where every kilogram is heated and cooled daily
Melting range1,360–1,411 °CSolidus–liquidus
Thermal conductivity≈ 11.2 W/m·K at 20 °C; rising to ≈ 30 W/m·K near 1,000 °CLower than 600 at room temperature; both converge at high temperature
Specific heat≈ 448 J/kg·KUse the high-temperature value for furnace-cycle calculations; it rises with temperature
Thermal expansion (mean, 20–100 °C)≈ 13.8 ×10⁻⁶ /KSlightly higher than 600 — check dissimilar welds and expansion gaps on long fixtures
Electrical resistivity≈ 1.19 µΩ·m at 20 °CRelevant to heating-element and thermocouple-sheath design
Modulus of elasticity≈ 206 GPa at 20 °CFalls sharply above 800 °C — the usual cause of sag in unsupported furnace fixtures
Magnetic behaviourNon-magnetic (relative permeability ≈ 1.005)Stays austenitic throughout the service range; no magnetic transformation to design around

Oxidation, carburisation and corrosion behaviour

Oxidation in air

Continuous service to about 1,180 °C, with intermittent service capability close to that because the alumina scale does not spall on cooling the way a chromia scale does. The mechanism matters for the design: the Al₂O₃ layer grows more slowly than Cr₂O₃, so metal loss over a 5-year campaign is much lower than for 600 at the same temperature. In clean oxidising atmospheres 601 is the most cost-effective nickel alloy above 1,000 °C.

Atmosphere limits — the part buyers get wrong

  • Reducing atmospheres (H₂, CO-rich, cracked ammonia): the alumina film cannot form. Above roughly 800 °C in strongly reducing gas, 601 is not protected and the duty belongs to a different family.
  • Sulphur-bearing gases: 601 tolerates moderate sulphidation better than 600 thanks to its higher chromium, but heavy sulphur at high temperature still attacks the scale. Check the sulphur partial pressure before committing.
  • Carburising atmospheres: good resistance — 601 is a standard choice for carburising furnace muffles and retorts, and for the internals of endothermic gas generators.
  • Thermal cycling: 601's strongest suit. Where 600 develops a cracked, spalling scale after repeated cycles, 601 keeps a continuous film.

Aqueous corrosion

Adequate rather than outstanding. 601 resists nitric acid and many oxidising salt solutions, and it is immune to chloride stress-corrosion cracking. It has essentially no molybdenum, so its PREN is only about 21–25: it is not a seawater, hypochlorite or wet-chloride alloy. It is also not intended for hot concentrated sulphuric or hydrochloric acid.

Selection rule of thumb: 601 wins when the failure mode is oxidation, carburisation or thermal-cycling spallation above 900 °C in an oxidising atmosphere. Below about 800 °C in wet corrosive service, or in caustic, 600 does the job for less. In seawater or chloride pitting duty, neither 600 nor 601 is right — that is 625 or super duplex territory.

Typical applications by industry

IndustryTypical 601 componentsWhy 601
Heat treatmentMuffles, retorts, furnace rollers, trays, baskets, fixtures, quench racks, radiant tubesOxidation resistance to 1,180 °C plus cycling tolerance — the classic 601 duty
Petrochemical / refiningReformer and cracker tube hangers, thermowells, heater supports, catalyst support gridsScale stability and creep strength in the 900–1,100 °C band
Chemical / fertiliserAmmonia oxidation catalyst gauze supports, nitric acid catalyst baskets, burner nozzlesOxidation resistance in ammonia and nitrous-gas environments
Power generationBoiler tube hangers, soot-blower parts, gas-turbine exhaust components, ignitersStrength and scaling resistance under cyclic thermal load
Environmental / wasteWaste-incinerator superheater supports, thermal-oxidiser internals, flue dampersTolerance of high-temperature combustion gas with moderate sulphur
Automotive / aerospaceExhaust manifolds and liners, turbocharger housings, afterburner components, spark-plug bodiesCyclic oxidation resistance at 950–1,100 °C
Glass & ceramicsGlass-melt electrodes, kiln furniture, kiln rollers, saggersNon-wetting, non-scaling at kiln temperature

Standards and product forms we supply

Product formStandardTypical supply range
Plate, sheet, stripASTM B168 / ASME SB168; AMS 58700.5–60 mm plate; sheet and coil to width
Bar, rod, wireASTM B166 / ASME SB166; AMS 5715Dia 8–250 mm bar; wire and rod to drawing
Seamless pipe and tubeASTM B167 / SB167Pipe to schedule; tube to drawing
Welded tube and pipeASTM B516 / B517Thin-wall and large-diameter sections
Fittings and forgingsASTM B366 / B564Butt-weld fittings, forged flanges and blocks
Weld consumablesERNiCr-3 (AWS A5.14); ENiCrFe-3 (AWS A5.11)Matching filler for 601-to-601 and dissimilar joints

Designations: UNS N06601 / W.Nr 2.4851 / NiCr23Fe / AFNOR NC 23 Fe / JIS NCF 601 / GB NS313 (cross-reference only). European coverage for heat-resisting service is EN 10095; flat-product standards are DIN 17750 and ISO 6208; VdTÜV material data sheet 305 covers pressure-retaining use in Germany.

Fabrication, welding and purchasing notes

Heat treatment

  • Solution anneal at 1,100–1,180 °C and cool quickly. Keep the soak short: 601 is prone to grain growth, and coarse grain costs ductility and low-cycle fatigue life.
  • Do not anneal in the 600–900 °C band for stress relief unless the application demands it — that is where aluminium-related precipitation starts and ductility drops.
  • Furnace atmosphere matters more than the number on the controller: sulphur or reducing gas during anneal will damage the surface scale that the alloy depends on.

Forming and machining

  • Hot working: 1,050–1,200 °C, finish above 900 °C, then anneal. Cold forming is possible but the work-hardening rate is high — expect intermediate anneals on deep draws.
  • Machining: carbide tooling, low speed, heavy feed, rigid set-up. The alloy is gummier than 600 and will work-harden under a dull edge.

Welding

  • No preheat, no post-weld heat treatment required for most service. Use ERNiCr-3 (FM 82) filler, or ENiCrFe-3 (WE 182) electrodes for covered-electrode work.
  • The aluminium content makes the pool slightly less fluid — use a slightly wider groove, keep interpass below 150 °C, and purge tube roots properly.
  • Post-weld cleaning: pickle and passivate (HF/HNO₃) to remove the chromium-depleted and alumina-contaminated surface layer; mechanical brushing alone is not enough on a heat-resistance alloy.
  • For furnace fixtures, design the weld away from the hottest zone where possible — weld metal and HAZ always have slightly lower creep life than the parent plate.

Purchasing checklist

  • Specify the standard and the condition (annealed, ASTM B168 or AMS 5870) — “Inconel 601” on its own leaves the mechanicals open.
  • Ask for the aluminium content on the certificate. It should sit inside 1.0–1.7 %; a heat at the bottom of the range is legal but will scale faster in cycling service.
  • Request grain size for furnace furniture and any part that will be thermally cycled.
  • PMI every piece. 601, 600 and 690 look identical, feel identical and are all non-magnetic — only chemistry separates them.
  • For pressure-retaining plate, confirm the ASME SB168 package before the mill rolls it; adding a U-stamp traceability dossier later is slow and expensive.

Buying Inconel 601 from Hangbo

We supply Inconel 601 plate, sheet, bar, seamless tube, welded tube, forged blanks and weld wire, cut and machined in Shanghai. Because 601 is usually bought for furnace furniture and heat-treat fixtures, most of our shipments are cut-to-size blanks or laser-cut profiles rather than random plate — send the flat pattern and we will quote the nest.

Every order ships with an EN 10204 3.1 certificate showing the actual heat analysis including aluminium, plus PMI verification on 100 % of pieces. Typical lead times: 10–20 days for stock plate, 25–35 days for cut and formed fixtures, 30–45 days for forged or machined parts. Tell us the atmosphere and the cycle — temperature, time at temperature, cooling method — and we will confirm whether 601 is the right grade or whether 600, 625 or a cast heat-resistant alloy will give you a longer campaign for less.

Frequently asked questions

Why does Inconel 601 resist oxidation better than 600?

Because of the aluminium. 601 contains 1.0–1.7 % Al, which oxidises preferentially and forms a dense, slow-growing Al₂O₃ scale. Alumina grows roughly an order of magnitude more slowly than chromia, and — the practical point — it stays adherent through heating and cooling cycles instead of spalling. That is what lifts the continuous service ceiling from about 1,095 °C for 600 to about 1,180 °C for 601 and gives 601 its thermal-cycling reputation.

What is the maximum service temperature of Inconel 601?

About 1,180 °C in continuous service in air, and close to that for intermittent service. Three conditions reduce it sharply: reducing atmospheres (the alumina cannot form, so the ceiling drops to roughly 800 °C), sulphur-bearing gases, and any mechanical load — above about 900 °C the alloy is carrying almost no useful stress, so the part must be supported by the design, not by the material.

Inconel 601 or 600 for a furnace muffle?

601, unless the furnace atmosphere is reducing or heavily sulphidising. For an oxidising or carburising muffle cycling between 900 and 1,100 °C, 601's alumina scale will outlast 600 by a wide margin. If the muffle runs below about 900 °C in clean gas, 600 is cheaper and perfectly adequate. If the gas is reducing above 800 °C, neither grade is protected — talk to us about a different family.

Can Inconel 601 be used in seawater or chloride service?

No. 601 has essentially no molybdenum, so its pitting resistance equivalent is only around 21–25 and it will pit and crevice-corrode in seawater, brine or hypochlorite. It is immune to chloride stress-corrosion cracking, which is a different mechanism. For seawater or wet chlorides, specify 625 (PREN ≈ 50) or a super duplex such as 2507.

Does Inconel 601 require post-weld heat treatment?

Generally no. Weld with ERNiCr-3 (FM 82) filler, keep interpass below 150 °C, and pickle/passivate the weld zone. Post-weld anneal at 1,100–1,180 °C is only needed where the design demands full parent-metal creep ductility in the HAZ, or where a cold-formed plus welded assembly will see severe thermal cycling — and it must be followed by a fast cool to avoid grain growth.

Need Inconel 601 (UNS N06601)?

Send us your drawing or specification for a quotation — we reply within one business day.

Request a quote