Inconel 718 (UNS N07718): composition, heat treatment and applications

Inconel 718 is the most-used age-hardenable nickel superalloy in the world: it carries the highest tonnage of any 1,300 MPa-class alloy in aerospace engines and oilfield tooling. Its trick is a slow age-hardening reaction (gamma-double-prime Ni₃Nb), which makes it remarkably weldable and crack-resistant for a high-strength grade — unusual company for a 1,240 MPa tensile alloy. This guide covers the numbers we quote against every day: composition, the standard double-ageing treatment, per-condition mechanicals and the machining traps to avoid.

Machined nickel alloy forged discs

What Inconel 718 is — in one paragraph

Inconel 718 (UNS N07718, W.Nr 2.4668) is a nickel-iron-chromium superalloy strengthened by precipitation of Ni₃Nb (gamma-double-prime) and a smaller Ni₃(Al,Ti) (gamma-prime) fraction. Roughly 50–55 % nickel, 17–21 % chromium, iron as balance, plus 2.8–3.3 % molybdenum and 4.75–5.5 % niobium. It retains useful strength from −250 °C (cryogenic) to about 700 °C — the gamma-double-prime phase resists coarsening unusually well, which is why 718 kept turbine-disc duty alive at temperatures where older gamma-prime alloys softened. It is supplied solution annealed and finishes its life after a double-ageing treatment in the customer's or forger's shop.

Nominal chemical composition

ElementContent (wt %)Why it matters
Nickel (Ni) + Cobalt (Co)50–55 (+1.0 Co max)Austenite matrix; controls the gamma-double-prime volume fraction
Chromium (Cr)17–21Oxidation and corrosion resistance to ~980 °C short excursions
Iron (Fe)balanceCost control and phase stability; keeps gamma-double-prime precipitation slow and manageable
Niobium + Tantalum (Nb+Ta)4.75–5.5The main strengthening element — forms Ni₃Nb
Molybdenum (Mo)2.8–3.3Solid-solution strengthening and creep resistance
Titanium (Ti)0.65–1.15Forms gamma-prime Ni₃(Al,Ti)
Aluminium (Al)0.2–0.8Forms gamma-prime; supports the ageing response
Carbon (C)0.08 maxCarbide control for weldability

The heat treatment: solution + double age

The standard AMS 5662 cycle that produces the 1,100–1,240 MPa class properties:

StepTemperature / timeCoolingPurpose
Solution anneal950–980 °C, 1 h (per AMS 5662 option: 980 °C)Air cool or fasterDissolves secondary phases, resets the grain structure
First age720 °C ± 10, 8 hFurnace cool ~55 °C/h to 620 °CNucleates fine gamma-double-prime
Second age620 °C ± 10, total 18 hAir coolGrows the precipitate to optimum size

Two supply conditions exist in practice: annealed (solution treated only, for further hot work or machining before final hardening) and aged / AMS 5662 (full treatment done — the condition for finished bars and discs). A 980 °C solution gives maximum strength with somewhat lower creep-rupture life; a 1,065 °C solution (AMS 5663 variant approach) trades a little yield for better creep and stress-rupture at 650 °C+.

Buying note: always state the required condition (annealed or aged per AMS 5662) and the test direction (longitudinal / transverse) on the PO — the same bar tested in the two conditions differs by more than 700 MPa in yield strength.

Mechanical properties

Minimum values per ASTM B637 / AMS 5662 (bars & forgings, aged, longitudinal):

ConditionYield strength (0.2 %)Tensile strengthElongationHardness
Solution annealed≈ 450–590 MPa≈ 830–900 MPa≥ 30–40 %≈ 180–240 HB
Aged (AMS 5662)≥ 1,034 MPa [1,080–1,200]≥ 1,276 MPa [1,350–1,450]≥ 12 % [15–20]≈ 36–44 HRC
Aged at 650 °C (typical retention)≈ 900–960 MPa≈ 1,150–1,200 MPa≈ 15 %—

The retention row explains 718's dominance: at 650 °C it still holds ~90 % of its room-temperature yield — competitors like A286 or 15-5 PH have fallen far below that.

Physical properties

PropertyValue
Density8.19 g/cm³
Melting range1,260–1,336 °C
Thermal conductivity (room temp)≈ 11.4 W/m·K
Thermal expansion (20–100 °C)≈ 13.0 ×10⁻⁶ /K
Elastic modulus (room temp)≈ 200 GPa
Magnetic behaviourEssentially non-magnetic

Typical applications

IndustryTypical 718 components
AerospaceJet-engine discs, spools, shafts, casings, fasteners; rocket-engine thrust chambers and turbopumps
Oil & gasDownhole tooling, drill collars, valve bodies, hanger and packer hardware in sour, high-pressure wells
PowerGas-turbine hot-section hardware, fasteners for high-temperature flanges
ToolingHigh-temperature die and extrusion tooling where H13 fails by softening

In oilfield service, 718 is the default high-strength choice for NACE MR0175 / ISO 15156 sour environments up to the hardness limit (HRC 40 per the standard's environmental restrictions) — we supply both standard and NACE-compliant heats, and the difference must be declared at order time.

Standards and product forms we supply

  • Bars / forgings: ASTM B637, AMS 5662 / 5663 / 5664
  • Plate / sheet / strip: AMS 5596 / 5597, ASTM B670
  • Seamless pipe & tube: AMS 5589 / 5590
  • Weld wire: ERNiFeCr-2 (AWS A5.14), AMS 5832
  • Forged rings, discs, blocks, machined parts: to drawing, EN 10204 3.1, ultrasonic tested to customer spec

Machining and welding notes

Machining: machine 718 in the solution-annealed condition whenever the part allows it, then age afterwards. Aged 718 machines at roughly 25–30 % of the speed of 316L — expect rapid notching on ceramic-free tooling; use positive-rake carbide, high pressure coolant, and avoid dwell. Work hardening is significant: keep the tool engaged and never let it rub.

Welding: the slow gamma-double-prime reaction is 718's superpower — weldments can be aged directly after welding without cracking risk that kills other high-strength superalloys. Use ERNiFeCr-2 filler (718 or 625 filler both acceptable for many joints), low heat input, and for critical parts follow weld with the full double-age to restore parent-metal strength.

Buying 718 from Hangbo

We supply Inconel 718 bar, forgings, rings, plate and machined parts in both annealed and fully aged condition, with EN 10204 3.1 certification, full traceability to the heat, and ultrasonic testing to customer specification. Forged rings and blocks can be supplied rough-machined or finish-machined to drawing. Typical lead time: 15–30 days for stock bar; 45–60 days for forged discs and rings with UT.

Frequently asked questions

Why is 718 so popular compared to other superalloys?

Three reasons: it welds without cracking (unlike Waspaloy or Rene 41), it holds strength to 700 °C (far above A286), and niobium replaced much of the cobalt — making it cheaper and supply-stable. That combination is why it carries the highest production tonnage of any superalloy.

What is the difference between AMS 5662 and AMS 5663?

Both cover 718 bar, but 5662 is the 966–996 °C solution + double age (maximum strength), while 5663 uses a higher solution temperature (~1,065 °C) for better creep-rupture life at 650 °C+. Specify the one your design was actually calculated against.

Can I machine 718 after ageing?

Yes, but at severely reduced cutting speeds and tool life. Standard practice is rough-machine in the annealed state, leave 0.5–1 mm grind/finish stock, age, then finish-machine or grind.

Is 718 suitable for sour oilfield service?

Yes, within NACE MR0175 limits — hardness must typically stay at or below HRC 40 and the environment's H₂S partial pressure and pH must be inside the standard's envelope. We can supply heats tested and certified for NACE compliance.