[email protected] WhatsApp +86 159 0085 2030 Qingpu, Shanghai Reply within 1 business day

Inconel 625 (UNS N06625): composition, properties and applications

Inconel 625 is the all-round workhorse of the nickel-molybdenum-chromium family: a solid-solution alloy strengthened by molybdenum and niobium that needs no post-weld heat treatment, resists pitting in seawater with a PREN of about 50, and stays strong from cryogenic temperature up to roughly 980 °C. This guide collects the numbers and the selection rules we use every day when quoting 625 plate, bar, pipe, forgings and weld overlay.

Machined nickel alloy forged discs

What Inconel 625 is — in one paragraph

Inconel 625 (UNS N06625, W.Nr 2.4856) is a nickel-base superalloy with 20–23 % chromium, 8–10 % molybdenum and 3.15–4.15 % niobium+tantalum. The molybdenum and niobium act together as solid-solution strengtheners, which is why 625 reaches higher strength than 600 or 601 without any ageing treatment. The high nickel content (58 % min) makes it essentially immune to chloride stress-corrosion cracking, and the combined Cr + Mo + Nb give it outstanding resistance to pitting and crevice corrosion — a PREN (pitting resistance equivalent number) of roughly 50, comparable to super duplex steels but without their toughness or weldability limits.

Nominal chemical composition

ElementContent (wt %)Why it matters
Nickel (Ni)58 minBaseline for chloride-SCC immunity and high-temperature stability
Chromium (Cr)20–23Oxidation resistance up to ~980 °C and general corrosion barrier
Molybdenum (Mo)8–10Pitting / crevice resistance and strength in reducing media
Niobium + Tantalum (Nb+Ta)3.15–4.15Solid-solution strengthening; stabilises the alloy (no sensitisation)
Iron (Fe)5 maxKeeps the fully austenitic structure
Carbon (C)0.10 maxLimits carbide precipitation in the weld HAZ
Manganese / Silicon0.5 max eachDeoxidation and processing control
Aluminium + Titanium0.4 maxDeliberately low — 625 is NOT an age-hardening grade in its standard form

For reference: a derivative grade, Inconel 625 with increased silicon (and the ™625LCF variant with controlled carbon), exists for specific fatigue and wet-corrosion duties — always confirm the exact variant on the purchase order.

Mechanical properties

Minimum values per ASTM B443 (Grade 1, annealed) with typical mill-certificate ranges in brackets:

ConditionYield strength (0.2 %)Tensile strengthElongation
Grade 1 — annealed (most common)≥ 414 MPa [480–620]≥ 834 MPa [900–1,100]≥ 30 % [35–45]
Grade 2 — solution treated (1,150 °C)≥ 345 MPa [390–520]≥ 760 MPa [820–950]≥ 30 % [40–50]

Notes for designers: Grade 1 (920–980 °C anneal) is the standard supply condition and the right choice for corrosion service. Grade 2 (solution treated at 1,150 °C) is specified when maximum creep-rupture strength above 650 °C matters more than room-temperature yield. 625 loses yield slowly with temperature — expect roughly 60 % of the room-temperature yield at 650 °C.

Physical properties

PropertyValue
Density8.44 g/cm³
Melting range1,290–1,350 °C
Thermal conductivity (room temp)≈ 9.8 W/m·K
Specific heat≈ 410 J/kg·K
Thermal expansion (20–100 °C)≈ 12.8 ×10⁻⁶ /K
Magnetic behaviourEssentially non-magnetic

Corrosion resistance — where 625 earns its keep

  • Seawater and brines: exceptional pitting and crevice resistance, virtually immune to chloride stress-corrosion cracking. Widely used uncoated in splash zones and subsea clamps.
  • Acids: very good in hydrochloric and sulfuric acid at low-to-moderate concentrations and temperatures; outperformed only by C-family alloys (C-276 / C-22) in hot, concentrated reducing acids.
  • Flue gas desulphurisation: a standard choice for scrubber internals, dampers and quench systems where sulphite/chloride condensates attack lesser alloys.
  • High temperature: oxidation resistant to about 980 °C; the niobium content also gives good carburisation resistance relative to simpler Ni-Cr grades.

Selection rule of thumb: if the medium is seawater or oxidising acid, 625 usually beats C-276 on price with comparable pitting resistance. If the medium is hot concentrated HCl or H₂SO₄, step up to Hastelloy C-276 / C-22 instead.

Typical applications

IndustryTypical 625 components
Oil & gas / subseaCladding (weld overlay) on risers and tree components, subsea fasteners, sour-service valve trim
Chemical processingHeat-exchanger tubing, reactor internals, transfer lines for mixed-acid service
AerospaceExhaust systems, thrust reverser components, turbine shrouds, bellows
MarinePropeller blades, submarine components, wire rope for mooring
Power / environmentalFGD scrubber internals, superheater tube hangers, nuclear waste handling

Standards and product forms we supply

  • Plate / sheet / strip: ASTM B443 / ASME SB443 (Gr.1 & Gr.2)
  • Bar / rod / forgings: ASTM B446 / ASME SB446, AMS 5666
  • Seamless pipe & tube: ASTM B444 / B829
  • Welded pipe & tube: ASTM B705 / B704
  • Weld wire / electrodes: ERNiCrMo-3 (AWS A5.14), ENiCrMo-3 (AWS A5.11)
  • Forged flanges, rings, blocks, machined parts: supplied to drawing with EN 10204 3.1 certificates

Welding and fabrication notes

625 is one of the easiest high-performance alloys to weld: no preheat, no post-weld heat treatment required for corrosion service, and the same ERNiCrMo-3 filler is used whether you are joining 625 to itself, to 825, or as overlay on carbon steel. Keep interpass temperature below 150 °C, use low heat input for the root pass, and pickling/passivating the weld area restores the full corrosion performance. For cold-formed parts, a stress-relief anneal (around 965 °C) is only required when the combination of deformation and medium makes re-sensitisation a design concern — in practice rarely for standard chloride service.

Buying 625 from Hangbo

We stock and process Inconel 625 plate, bar, seamless pipe, forgings and wire, with in-house saw cutting, turning, and weld-overlay capability. Every shipment goes out with EN 10204 3.1 mill certificates, and PMI verification is standard before packing. Typical lead time: 7–15 days for stock sizes, 30–45 days for forged or machined-to-drawing parts.

Frequently asked questions

Is Inconel 625 magnetic?

No — 625 is essentially non-magnetic in the annealed condition. A magnet response after heavy cold work is normal and does not indicate a wrong grade.

Can 625 be age hardened?

Standard 625 is a solid-solution grade and is not age hardened. The high-strength variants (625LS, 725) add ageing treatments — if your spec calls for 1,000+ MPa yield, you are probably looking at Alloy 725, not 625.

625 vs 825 — which should I buy?

825 (N08825) is cheaper and sufficient up to about 450 °C for sulfuric/phosphoric acid service. Choose 625 when you need the PREN ≈ 50 pitting resistance, seawater duty, or strength above 450 °C.

What is the price difference vs 316L?

Roughly 8–12× per kg depending on form and quantity — driven by the 58 %+ nickel and 8–10 % molybdenum content. For seawater service the lifecycle cost usually favours 625 once maintenance and replacement are counted.

Need Inconel 625 (UNS N06625)?

Send us your drawing or specification for a quotation — we reply within one business day.

Request a quote