Grade guides library: one technical page per alloy
Composition, properties, corrosion behaviour, applications and standards for each grade — Inconel 625, 718, Hastelloy C-276 and more, with new guides added every week.
Open the library200+ grades across five material families, supplied in the form and size your production needs. Filter by category below, or send us the specification you work to and we will confirm availability.
93 grades in regular supply — plus other grades, bespoke chemistries and mill-order quantities. Tell us what you work to and we will confirm.
Monel 404
Ni-CuN04404
Low-permeability Ni-Cu for RF shielding and electronic wire.
Per mill specification (wire, strip)
Monel 401
Ni-CuN04401
Specialty Ni-Cu for electronic hermetic sealing wire and low-Curie-temperature applications.
Per mill specification (wire, strip)
Hastelloy B-3
Ni-MoN10665 / 2.4600
Hydrochloric acid at all concentrations and temperatures with improved thermal stability versus B-2.
ASTM B333/B335/B622/B619/B626
Hastelloy G-30
Ni-Cr-Fe-MoN06030
High-chromium grade for wet-process phosphoric acid plants, HNO3/HF pickling and oxidising media.
ASTM B582/B581/B622/B619/B626
Hastelloy C-4
Ni-Cr-MoN06455 / 2.4610
Thermally stable C-type for post-weld service; wet-process phosphoric acid and HF environments.
ASTM B575/B574/B622/B619/B626
Hastelloy C-2000
Ni-Cr-Mo-CuN06200 / 2.4675
Versatile corrosion resistance in both reducing and oxidising acids; strong in HNO3/HF and mixed-acid service.
ASTM B575/B574/B622/B619/B626
Inconel 600
Ni-Cr-FeN06600 / 2.4816
General-purpose high-temperature alloy; resistant to chloride SCC and caustic
ASTM B166/B167/B168
Inconel 601
Ni-Cr-Fe-AlN06601 / 2.4851
Excellent oxidation and high-temperature scaling resistance up to ~1200 °C
ASTM B166/B168
Inconel 625
Ni-Cr-Mo-NbN06625 / 2.4856
High strength from cryogenic to ~980 °C; outstanding pitting and crevice resistance
ASTM B443/B446/B444, AMS 5666
Inconel 690
Ni-Cr-FeN06690 / 2.4642
Very high chromium; steam-generator tubing grade with superior SCC resistance
ASTM B166/B167/B163
Inconel 693
Ni-Cr-Fe-AlN06693 / 2.4650
Designed for metal-dusting resistance in reducing / oxidising high-temp service
ASTM B166/B167/B168
Inconel 718
Age-hardenable NiN07718 / 2.4668
High-strength age-hardenable alloy for −250 to 700 °C; aerospace workhorse
ASTM B637, AMS 5662/5663
Inconel X-750
Age-hardenable NiN07750 / 2.4669
High creep-rupture strength, relaxation resistance for springs and fasteners
ASTM B637, AMS 5667
Incoloy 800 / 800H
Fe-Ni-CrN08800 / N08810
Creep-resistant austenitic alloy for high-temperature process equipment
ASTM B409/B408
Incoloy 825
Ni-Fe-Cr-Mo-CuN08825 / 2.4858
Broad acid and chloride resistance; classic sulphuric and phosphoric acid duty
ASTM B424/B425/B423
Incoloy 925
Age-hardenable Ni-FeN09925 / 2.4852
High-strength sour-service grade for downhole tubular and wellhead hardware
ASTM B805, NACE MR0175
Monel 400
Ni-CuN04400 / 2.4360
Resistant to seawater, hydrofluoric acid and alkalis; good weldability
ASTM B127/B164/B165
Monel K-500
Age-hardenable Ni-CuN05500 / 2.4375
Monel 400 with added strength and hardness for pump shafts and valves
ASTM B865, QQ-N-286
Nickel 200 / 201
Commercially pure NiN02200 / N02201
High electrical and thermal conductivity with excellent caustic resistance
ASTM B162/B160/B161
Hastelloy C-276
Ni-Mo-CrN10276 / 2.4819
Broadest corrosion resistance for aggressive mixed acid and chloride media
ASTM B575/B574/B622
Hastelloy C-22
Ni-Cr-Mo-WN06022 / 2.4602
Enhanced resistance to oxidising media and pitting over C-276
ASTM B575/B574
Hastelloy B-2
Ni-MoN10665 / 2.4617
For hydrochloric and sulphuric acid service free of oxidising species
ASTM B333/B335
Alloy 20 (Carpenter 20Cb-3)
Ni-Fe-Cr-Mo-CuN08020 / 2.4660
Sulphuric acid and chloride duty; stabilised against intergranular attack
ASTM B463/B473/B729
904L
Super-austeniticN08904 / 1.4539
High Mo + Cu; resistant to dilute sulphuric and phosphoric acid and pitting
ASTM B625/B649, EN 10088
254SMO
Super-austenitic 6MoS31254 / 1.4547
PREN > 42; high resistance to chloride pitting and crevice corrosion
ASTM A240/A182, EN 10088
AL-6XN
Super-austenitic 6MoN08367
Seawater and process service where 316L and 317L fall short
ASTM A240/A182
Sanicro 28
Super-austeniticN08028 / 1.4563
Sulphuric and phosphoric acid service; excellent in wet-process phosphoric acid
ASTM B668/B709
317L
AusteniticS31703 / 1.4438
Higher Mo than 316L for improved acid and pitting performance
ASTM A240/A276
310S / 310H
Heat-resistant austeniticS31008 / 1.4845
High Cr-Ni for continuous service in oxidising atmospheres up to ~1100 °C
ASTM A240/A312
321 / 347 (H)
Stabilised austeniticS32100 / S34700
Ti or Nb stabilised for elevated-temperature and weld-adjacent service
ASTM A240/A312
2205
DuplexS32205 / S31803 / 1.4462
Yield ≈ 450 MPa; excellent SCC resistance in chloride media. The workhorse duplex
ASTM A240/A182/A790
2507
Super duplexS32750 / 1.4410
PREN > 40, yield ≈ 550 MPa; seawater and offshore topside systems
ASTM A240/A182/A789
2304
Lean duplexS32304 / 1.4362
Low-cost duplex alternative where 304/316 SCC resistance is insufficient
ASTM A240/A789
Zeron 100
Super duplexS32760 / 1.4501
Cu + W additions; highest pitting resistance in the duplex family
ASTM A182/A240
Ferralium 255
Super duplexS32550 / 1.4507
High strength with good wear resistance for pump and valve components
ASTM A182/A479
XM-25 / Custom 450
Martensitic PHS45000 / 1.4592
≈ 2× the yield of 316 with good corrosion resistance; easy to machine and weld
ASTM A564, AMS 5773
17-4 PH
Martensitic PHS17400 / 1.4542
The most widely used PH grade; range of ageing temperatures for strength / toughness balance
ASTM A564, AMS 5643
15-5 PH
Martensitic PHS15500 / 1.4545
17-4 PH performance with improved transverse toughness and forgeability
ASTM A564, AMS 5659
Custom 455
Martensitic PHS45500
Very high strength with good ductility; aerospace fasteners and actuators
ASTM A564, AMS 5617
13-8 Mo
Martensitic PHS13800
High strength with superior toughness and SCC resistance in the PH family
ASTM A564, AMS 5629
17-7 PH
Semi-austenitic PHS17700 / 1.4568
Spring and diaphragm grade supplied in strip and wire
ASTM A693, AMS 5528
A286
Fe-Ni-Cr, age-hardenableS66286 / 1.4980
High-temperature bolting and turbine hardware to ~700 °C
ASTM A453, AMS 5731
Nimonic 80A
Ni-Cr, age-hardenableN07080 / 2.4952
High-temperature strength for exhaust valves and turbine parts
BS HR 2, AMS 5828
Nimonic 90
Ni-Cr-CoN07090 / 2.4632
Higher creep strength than 80A for turbine blades and discs
AMS 5827, BS HR 501
Titanium Gr.2
Commercially pure TiR50400
Excellent seawater and oxidising-acid resistance at low density
ASTM B265/B348
Titanium Gr.5 (Ti-6Al-4V)
Ti alloyR56400
High specific strength; aerospace and medical structural parts
ASTM B348, AMS 4928
Zirconium 702
Reactive metalR60702
Nuclear-grade corrosion resistance to hot organic and mineral acids
ASTM B551/B523
Nickel 200 strip / mesh
Pure Ni, fabricatedN02200
Catalyst gauze, electrodes and battery hardware in fine strip and mesh
ASTM B162/B160
2507 Weld Consumables
Filler metalER2594 / E2594
Matching filler wire and electrodes for super duplex fabrication
AWS A5.9 / A5.4
Haynes 188
Co-Ni-Cr-WR30188
Combustion liners, transition ducts and afterburner parts to 1100 °C; excellent oxidation and hot-corrosion resistance.
AMS 5608/5609, AMS 5772
Haynes 25 (L-605)
Co-Cr-W-NiR30605
Turbine blades, bearing races, fasteners and springs in service up to 980 °C.
AMS 5759, AMS 5537
Waspaloy
Ni-Cr-Co-Mo-Ti-AlN07001 / GH4738
Gas-turbine blades, discs and bolts to 870 °C; Chinese designation GH4738.
ASTM B637, AMS 5704/5706/5708/5709
Rene 41
Ni-Cr-Co-Mo-Ti-AlN07041 / GH4141
Turbine discs, blades and bolts in 870–980 °C service; Chinese designation GH4141.
AMS 5661/5545, ASTM B637
Incoloy 901
Ni-Fe-Cr-Mo-TiN09901 / GH2901
Engine shafts, discs and rings to 650 °C; Chinese designation GH2901.
ASTM B637, AMS 5660/5661
GH3030
Ni-Cr solid solution80Ni-20Cr (≈ Nimonic 75)
Combustion liner and afterburner sheet parts to 800 °C; Chinese 80Ni-20Cr solid-solution grade.
GB/T 14992, GJB 1952
GH3039
Ni-Cr-Mo-NbNi-Cr-Mo-Nb
Flame tubes and cold-welded combustor parts to 900 °C.
GB/T 14992, GJB
GH3128
Ni-Cr-W-MoNi-Cr-W-Mo
Flame tubes, guide vanes and combustor parts to 950 °C; dual W+Mo solid-solution strengthening.
GB/T 14992
GH3044
Ni-Cr-WNi-Cr-W (ЭИ868)
Flame tubes and furnace fixtures; long-term to 900 °C, short-time oxidation to 1100 °C.
GB/T 14992
GH4049
Ni-Co-CrNi-Co-Cr-W-Mo (ЭИ867)
850–950 °C turbine blades and hot-section parts; among the strongest wrought Ni grades at 900 °C.
GB/T 14992, GJB
GH698
Ni-Cr-Mo-Nb-Ti-AlЭИ698 (XH73MБTЮ)
Turbine discs, compressor discs, retaining rings and fasteners at 750–800 °C.
GB/T 14992, GJB 3782
Titanium Gr.1
CP TitaniumR50250 / TA1
Most ductile CP titanium for chemical equipment and lined vessels.
ASTM B265/B338/B348
Titanium Gr.9
Ti-3Al-2.5VR56320 / TA18
Hydraulic tubing, bicycle frames and sporting goods; strength above CP grades with cold formability.
ASTM B265/B338/B348
Titanium Gr.12
Ti-0.8Ni-0.3MoR53400 / TA10
Chemical shell-and-tube exchangers with improved crevice corrosion resistance.
ASTM B265/B338/B348
304 / 304L
AusteniticS30400 / S30403
The universal austenitic grade for food, chemical and architectural service; 304L for post-weld corrosion; GJB military variants available.
ASTM A240/A312/A276
316L
Austenitic MoS31603 / 1.4404
Marine, chemical and pharmaceutical equipment with chloride pitting resistance.
ASTM A240/A312/A276, EN 1.4404
301
AusteniticS30100 / 1.4310
High-strength temper-rolled strip for springs and structural cladding.
ASTM A240/A666
309S
Austenitic heat-resistingS30908
Furnace parts and exhaust systems under intermittent high-temperature service.
ASTM A240/A312
314
Austenitic heat-resisting SiS31400
Furnace fixtures, radiant tubes and refractory anchors with high-Si scaling resistance.
ASTM A240/A276
1.4841 (2520Si2)
Austenitic heat-resistingEN 1.4841
Cement kilns, furnace rollers and heat-treatment fixtures to 1050 °C.
EN 10088-1
Alloy 926 (1.4529)
Super austenitic 6MoN08926 / 1.4529
FGD scrubbers, seawater and brine handling; 6 % Mo upgrade of 904L.
ASTM B625/B673/B674/B675/B676
XM-27
Fe-Ni-Cr-MoN08027
Wet-process phosphoric acid and FGD service; high-chromium 6Mo austenitic.
Per mill certificate (check applicable spec)
410
MartensiticS41000 / 1.4006
Hardenable martensitic for pump shafts, valves and turbine parts.
ASTM A240/A276
420
MartensiticS42000 / 1.4021
Cutlery, surgical instruments and valve internals.
ASTM A240/A276
3Cr13 (1.4028)
Martensitic1.4028
Cutlery and hardened components with higher carbon than 2Cr13.
EN 10088, GB/T 1220
4Cr13 (1.4034)
Martensitic1.4034
Plastic moulds and hardened wear parts.
EN 10088, GB/T 1220
430
FerriticS43000 / 1.4016
Nickel-free ferritic for appliance trim and kitchen equipment.
ASTM A240/A276
431
MartensiticS43100 / 1.4057
Marine shafts, nuts and bolts with corrosion resistance above 410.
ASTM A276
416
Martensitic free-machiningS41600 / 1.4005
Free-machining shafts, screws and valve parts.
ASTM A582/A276
444
Ferritic 2MoS44400 / 1.4521
Solar thermal tanks, hot-water heaters and exhaust parts with chloride pitting resistance.
ASTM A240/A268
440C
Martensitic high-CS44004
Bearing balls, valve seats and knife blades.
ASTM A276/A240
440F
Martensitic free-machiningS44020
Free-machining high-hardness components.
ASTM A582
15-7 PH
PH austeniticS15700
Springs, diaphragms and aircraft panels needing high strength with moderate corrosion resistance.
ASTM A693, AMS 5520
30CrMnSiA
Cr-Mn-Si structuralGB 30CrMnSiA
Aviation structural parts and high-strength bolts.
GB/T 3077, GJB
30CrMnSiNi2A
Cr-Mn-Si-Ni structuralGB 30CrMnSiNi2A
Landing gear and high-load aircraft structural forgings.
GB/T 3077, GJB
35CrMnSiA
Cr-Mn-Si structuralGB 35CrMnSiA
High-strength shafts and connecting rods.
GB/T 3077
T1 HSS (W18Cr4V)
Tungsten HSSASTM A600 T1
General-purpose tungsten high-speed steel cutting tools.
ASTM A600
M2 HSS (W6Mo5Cr4V2)
Mo HSSASTM A600 M2
Drills, taps, end mills and saws (Chinese 6542).
ASTM A600
M35 HSS (W6Mo5Cr4V2Co5)
Co HSSASTM A600 M35
High-performance HSS tools for hard and abrasive steels (SKH55).
ASTM A600
M4 HSS
High-V HSSASTM A600 M4
Heavy-duty broaches and cold-work tools.
ASTM A600
DC53
Cold-work die steelDaido DC53
Cold-work dies with double the toughness of D2.
Daido DC53 / JIS-equivalent
D2 (1.2379)
Cold-work die steelASTM A681 D2 / EN 1.2379
Cold-work dies, blanking and forming tools (SKD11, DC11).
ASTM A681, EN 1.2379
1.2510 (2510)
Oil-hardening steelEN 1.2510
Small dies, gauges and wood-cutting tools (SKS3-type).
EN ISO 4957
H13 (1.2344)
Hot-work die steelASTM A681 H13 / EN 1.2344
Hot-work dies, die-casting dies and extrusion tooling (SKD61).
ASTM A681, EN 1.2344
No grade matches that search. Send us the specification you work to and we will confirm availability.
Grades listed above are indicative of our regular range. Material can also be supplied to customer purchasing specifications, third-party-approved specifications, and NACE MR0175 / ISO 15156 sour-service requirements.
Ranges below cover our standard supply. Sizes outside these limits are usually available on mill order — tell us what you need.

0.5 – 200 mm thick

Ø 5 – 500 mm

6 – 120 mm across flats

OD 6 – 219 mm · WT 0.8 – 25 mm

OD 12 – 610 mm

Ø 0.8 – 8.0 mm

0.05 – 3.0 mm thick

To drawing · up to 3,000 kg

DN 15 – 600 · SCH 10 – 160

DN 15 – 600 · LR & SR

DN 15 – 600 · any combination

M6 – M100 · 1/4" – 4"

Up to Ø 3,000 mm × 500 mm

Waterjet / plasma / laser / CNC
Practical guides on grade selection, corrosion behaviour and sourcing — written by the people who quote and ship these alloys every day.
Composition, properties, corrosion behaviour, applications and standards for each grade — Inconel 625, 718, Hastelloy C-276 and more, with new guides added every week.
Open the library
The three famous brand names cover very different alloys. Which family fits which corrosion or temperature problem — and the selection rules that keep you out of trouble.
Read article
Price per kg is the least informative number in a quotation. How to qualify a supplier: traceability, honest heats, the documents to demand — and the red flags to walk away from.
Read articleIt depends on the grade and the product form. Mill-finished specialty grades (for example N06693) are produced to order with a per-ton minimum; commonly stocked nickel alloys and stainless grades can start from around 100 kg. We always state the MOQ upfront, before we quote.
ASTM, ASME, AMS, EN, DIN, JIS and GB are all routine. Tell us the standard and the revision year with your enquiry — the mill test certificate will be issued against the standard you specify.
Standard terms are 30 % T/T deposit with the balance against the copy of the bill of lading. For larger orders, payment terms can be negotiated between both parties (e.g. irrevocable L/C at sight). New customers start with standard terms; there is no hidden surcharge for first orders.
Samples are charged. Small material coupons for analysis or testing are billed at cost, and you also cover the courier cost. Machined sample parts are quoted case by case depending on the processing involved.
Send us the operating conditions — medium, temperature, pressure, standard — and we will recommend a grade and price it.