Inconel 693 (UNS N06693): the alloy built against metal dusting — composition, properties and applications

Inconel 693 is the industry reference grade against metal dusting — the aggressive carburisation failure that destroys Alloy 600, 601, 800H and even 625 parts in CO/H₂-rich syngas service. By pairing the same ~29 % chromium as 690 with about 3 % aluminium, 693 forms a protective alumina film precisely in the reducing atmospheres where chromia scales break down. Recommended service window for dusting duty is roughly 538–760 °C, with oxidation resistance to about 1,200 °C. This guide covers the composition, properties, selection logic and supply standards — 693 is a made-to-order grade at Hangbo, produced on a mill basis per ton.

Machined nickel alloy forged discs

What Inconel 693 is — in one paragraph

Inconel 693 (UNS N06693, EN 2.4650) is a nickel-base alloy with roughly 60.5 % nickel, 29 % chromium and 3 % aluminium, developed by Special Metals as the metallurgical successor to 690 for high-temperature corrosive service. The chromium gives it oxidation and sulfidation resistance on par with 690; the aluminium addition is what sets it apart — in the reducing, carbon-active atmospheres typical of syngas plants, aluminium preferentially forms a stable α-Al₂O₃ scale that chromia-forming alloys cannot maintain. The result is the best metal-dusting resistance of any commercially established nickel alloy, which makes 693 the default answer when thermowells, baffles, valve trim or furnace fixtures keep failing in reformer and SNG service.

Nominal chemical composition

ElementContent (wt %)Why it matters
Nickel (Ni)balance (≈ 60.5 nominal)Austenitic base; carburisation resistance and high-temperature strength
Chromium (Cr)27.0–31.0Protective Cr₂O₃ scale; oxidation and sulfidation resistance
Aluminium (Al)2.5–4.0The signature element — α-Al₂O₃ film under reducing carburising atmospheres; suppresses metal dusting
Iron (Fe)2.5–6.0Controlled narrow band to preserve austenite stability and high-temperature strength
Niobium (Nb)0.5–2.5Solid-solution strengthening; stable NbC fixes carbon away from grain boundaries
Titanium (Ti)1.0 maxResidual/secondary carbide former
Carbon (C)0.15 maxControlled carbide formation without heavy sensitisation
Manganese (Mn)1.0 maxDeoxidation and sulfur control
Silicon (Si)0.5 maxProcessing control

Mechanical properties

693 is supplied solution annealed (about 1,100–1,200 °C followed by rapid cooling). Typical mill values — since widely published minimums are limited for this grade, always confirm the required minimums on the purchase order:

Condition / formYield strength (0.2 %)Tensile strengthElongation
Hot-rolled + annealed plate (typical)≈ 490 MPa≈ 883 MPa≈ 45 %
Cold-drawn + annealed tube (typical)≈ 530 MPa≈ 937 MPa≈ 42 %
Bar, annealed (typical)310–480 MPa760–860 MPa35–45 %

Design notes: strength is retained well at temperature — 693 keeps useful creep-rupture properties up to about 980 °C and outperforms Alloy 601 in the 700–900 °C range. Modulus of elasticity is approximately 215 GPa at room temperature. Heavy sections for critical dusting service can be sourced with premium melt practice (e.g. electroslag remelting) — flag this in the RFQ.

Physical properties

PropertyValue
Density7.77 g/cm³
Melting range1,317–1,367 °C
Thermal conductivity (room temp)≈ 12.5 W/m·K
Specific heat≈ 460 J/kg·K
Thermal expansion (20–1,000 °C, mean)≈ 13.5 ×10⁻⁶ /K
Electrical resistivity≈ 1.17 µΩ·m
Magnetic behaviourEssentially non-magnetic

Metal dusting and high-temperature corrosion resistance

  • Metal dusting: this catastrophic form of carburisation injects carbon into the metal surface in CO/H₂-rich atmospheres between roughly 450 and 800 °C, producing pitting, dust and thin-wall failure within months. 693's alumina film blocks the mechanism and it shows the best resistance of any established nickel alloy — far ahead of 600, 601, 800H and 625 in the same environment.
  • Carburisation (general): deep carburising case growth is drastically slowed; typical service life of 693 thermowells and furnace hardware in carburising atmospheres is a multiple of 601/800H equivalents.
  • Oxidation: excellent in air up to about 1,100 °C, with short excursions to 1,200 °C tolerated without scale spallation.
  • Sulfidation: good in both oxidising and reducing sulfur-bearing atmospheres — relevant for coal gasification and waste-derive fuel plants.
  • Wet corrosion: the high Cr content gives solid behaviour in oxidising media, but 693 is not the answer for hot reducing acids — that is C-family territory.

Selection rule of thumb: design window for metal-dusting service is roughly 538–760 °C (1,000–1,400 °F). If your part fails by dusting in syngas, reformer or SNG duty, 693 is the grade. If the medium is liquid hot acid instead, move to Hastelloy C-276/C-22. If only oxidation matters, 601 reaches higher temperatures at lower cost.

Typical applications

IndustryTypical 693 components
Syngas / SNG / hydrogenThermowells and thermocouple protection tubes, baffles, transfer-line hardware in CO/H₂ streams
Steam reforming (methanol, ammonia, hydrogen plants)Reformer outlet fittings, pigtail and manifold hardware, catalyst-tube supports
Coal gasificationInternals and instrument fittings in reducing, sulfur-bearing gas
Heat treatmentCarburising-furnace fixtures, retorts, roller rails, radiant tubes
Refining / petrochemicalValve trim, reactor internals exposed to carbon-active streams
Glass / oxide-melt contactHardware in oxide-rich melts and frit environments up to 1,100 °C

Standards and product forms we supply

  • Bar / rod / wire: ASTM B166
  • Seamless pipe & tube: ASTM B167
  • Plate / sheet / strip: ASTM B168 (general requirements ASTM B906)
  • Welded fittings: ASTM B366
  • Aerospace procurement: AMS 5932
  • Weld wire: ERNiCrFeAl-1 (AWS A5.14) — matching composition, so the weld metal carries the same dusting resistance
  • Forgings, rings, thermowells machined from bar: supplied to drawing with EN 10204 3.1 certificates

Supply note: 693 is not a running stock item for most mills — expect production-based orders. Hangbo supplies it on a made-to-order, per-ton mill basis with defined lead times agreed at quotation.

Welding, fabrication and purchasing notes

Weld with the matching ERNiCrFeAl-1 filler — do not substitute generic 600-family fillers (ERNiCrFe-6/-7 or ERNiCrMo-3), because a weld metal without aluminium loses the dusting resistance that justified choosing 693 in the first place. No preheat is required; keep interpass temperature below 150 °C and use low heat input. Where the assembly serves dusting duty, a post-weld solution anneal (about 1,100 °C + rapid cool) restores the uniform structure and is strongly recommended for thermowell tips and thin sections. For machining, expect behaviour like other high-Cr nickel alloys: rigid setups, sharp positive-rake carbide tooling, and generous coolant flow. On purchasing: confirm product form (B166/B167/B168), condition (solution annealed), minimum mechanicals, certificate type (EN 10204 3.1) and any premium melt requirement at RFQ stage — 693 is produced per order, so every one of these parameters is locked at the mill booking, not negotiated afterwards.

Buying 693 from Hangbo

Inconel 693 is a made-to-order grade at Hangbo — we do not run it as standing stock. Orders are placed with the mill on a per-ton production basis (bar, plate, seamless pipe, forgings or machined thermowells), typically with 60–90 day lead times depending on form and melt practice. Every shipment leaves with EN 10204 3.1 mill certificates, PMI verification, and heat-treatment charts when solution annealing is specified. Send us the drawing, the gas analysis of your stream and the failure history of the parts it replaces — that is the fastest route to a correct 693 quotation.

Frequently asked questions

What is metal dusting, exactly?

A form of carburisation occurring in CO/H₂-rich gases between roughly 450 and 800 °C: carbon deposits on the surface, injects into the metal, and the affected zone disintegrates into graphite-rich dust and pits. Failures can occur within months. Conventional chromia-forming alloys (600, 601, 800H, 625) all suffer; 693's alumina film is what stops it.

Can I use 693 above 800 °C?

Yes, but the reason changes. Above the dusting window (538–760 °C recommended), 693 serves as an oxidation/sulfidation-resistant alloy with good strength to about 980 °C and oxidation resistance to 1,100–1,200 °C. If your duty is purely oxidising with no carburising risk, 601 or 800H is usually more economical.

Why is aluminium the key element in 693?

In reducing, carbon-active atmospheres, the Cr₂O₃ scale that protects ordinary alloys becomes unstable. Aluminium has a stronger affinity for oxygen than chromium and forms α-Al₂O₃ — a slow-growing, tenacious film that remains protective exactly where chromia fails. With ~3 % Al, 693 maintains that film in syngas conditions.

Is 693 available from stock?

Rarely. 693 is a specialist mill-produced grade; at Hangbo it is supplied made-to-order on a per-ton production basis with agreed lead times (typically 60–90 days). If your project needs it, get the mill booking started early.

Need Inconel 693 (UNS N06693)?

Send us your drawing or specification for a quotation — we reply within one business day.

Request a quote