Open the listIncoloy 800HT is the top rung of the 800-series ladder: same Fe-Ni-Cr base as 800 and 800H, but with aluminium + titanium forced into a tight 0.85–1.20 % window and a special coarse-grain solution anneal above 1,149 °C. Those two controls are what buy its higher creep-rupture strength in long service above 700 °C — exactly the regime of hydrogen-reformer manifolds and ethylene-cracker tubes. This guide sets out the composition differences, the property data, and the procurement checks that keep you from receiving 800H material on an 800HT order.
Incoloy 800HT (UNS N08811, W.Nr 1.4959, EN X8NiCrAlTi32-21) is a nickel-iron-chromium alloy (about 30–35 % Ni, 19–23 % Cr, iron balance) engineered specifically for creep-controlled service above roughly 600 °C. Compared with Incoloy 800H it adds two tighter controls: the combined aluminium + titanium content must fall in the 0.85–1.20 % window (800H merely requires Al+Ti ≥ 0.30 % with 0.15–0.60 % each), and the material must be solution annealed at 1,149 °C minimum to develop a coarse grain structure (ASTM No. 5 or coarser). In long service at 650–850 °C the titanium and aluminium drive formation of fine γ′ precipitates and stable carbides that pin grain boundaries and resist dislocation motion — the mechanism behind 800HT's higher creep-rupture life than 800H in furnace tubing and reformer headers.
Limits per ASTM B407/B409-family specifications (values per UNS N08811 as quoted across producer data sheets):
| Element | 800HT (N08811) | 800H (N08810) | Why it matters |
|---|---|---|---|
| Nickel (Ni) | 30.0–35.0 | 30.0–35.0 | Austenite stabiliser; chloride-SCC resistance |
| Chromium (Cr) | 19.0–23.0 | 19.0–23.0 | Cr₂O₃ protective scale; oxidation and carburisation resistance |
| Iron (Fe) | balance (≥ 39.5) | balance (≥ 39.5) | Cost-effective matrix; keeps the grade far cheaper than full Ni alloys |
| Carbon (C) | 0.06–0.10 | 0.05–0.10 | Controlled for grain-boundary carbides that aid creep strength |
| Aluminium (Al) | 0.25–0.60 | 0.15–0.60 | γ′ former — the raised lower bound is one half of the 800HT differentiator |
| Titanium (Ti) | 0.25–0.60 | 0.15–0.60 | γ′ former and carbide stabiliser |
| Al + Ti combined | 0.85–1.20 | 0.30–1.20 (min 0.30) | The key differentiator — guarantees every heat has enough Al+Ti for precipitation strengthening |
| Manganese / Silicon | ≤ 1.50 / ≤ 1.00 | ≤ 1.50 / ≤ 1.00 | Deoxidation and processing control |
| Copper / Sulfur | ≤ 0.75 / ≤ 0.015 | ≤ 0.75 / ≤ 0.015 | Residual control |
800, 800H and 800HT share one Fe-Ni-Cr base — the grades differ only in carbon window, Al+Ti window and mandatory grain size / anneal temperature. PMI cannot reliably separate them: the acceptance evidence lives on the mill certificate (UNS number, Al+Ti sum, grain-size note), so the certificate — not the chemistry stamp — is what you audit.
Room-temperature minima in the solution-annealed condition per ASTM B409/B407/B408 (N08811), with typical mill values in brackets:
| Condition | Yield strength (0.2 %) | Tensile strength | Elongation |
|---|---|---|---|
| Solution annealed — specification minimum (plate / bar / tube) | ≥ 170 MPa | ≥ 450 MPa | ≥ 30 % |
| Typical annealed plate | [≈ 200] | [≈ 530] | [≈ 52] |
| Typical hardness | ≈ 126 HB (annealed) | ||
Representative short-time elevated-temperature tensile values (typical annealed material, converted from producer data):
| Temperature | Tensile strength | Yield strength (0.2 %) | Elongation |
|---|---|---|---|
| 538 °C (1,000 °F) | ≈ 438 MPa | ≈ 114 MPa | ≈ 51 % |
| 649 °C (1,200 °F) | ≈ 384 MPa | ≈ 102 MPa | ≈ 50 % |
| 760 °C (1,400 °F) | ≈ 223 MPa | ≈ 99 MPa | ≈ 78 % |
| 871 °C (1,600 °F) | ≈ 128 MPa | ≈ 80 MPa | ≈ 120 % |
For design, creep rupture is what matters. Representative 10,000-hour rupture strengths are roughly 50 MPa at 760 °C and 24 MPa at 871 °C, with 100,000-hour rupture of the order of 120 MPa at 650 °C and 50 MPa at 760 °C. ASME Section VIII design allowables for N08811 extend to about 899 °C (1,650 °F) — the whole point of the grade. The elevated-temperature figures above are typical values for orientation; the governing design values must come from the applicable code tables.
| Property | Value |
|---|---|
| Density | 7.94 g/cm³ |
| Melting range | 1,357–1,385 °C (≈ 1,350–1,400 °C across sources) |
| Thermal conductivity (room temp / 100 °C) | ≈ 12 / ≈ 18 W/m·K |
| Specific heat (0–100 °C) | ≈ 460 J/kg·K |
| Thermal expansion (20–100 °C) | ≈ 14.4 ×10⁻⁶ /K (rising to ≈ 17.1 at 20–650 °C) |
| Modulus of elasticity (21 °C) | ≈ 196.5 GPa |
| Electrical resistivity | ≈ 1.01 µΩ·m |
| Magnetic behaviour | Austenitic; low permeability (≈ 1.01 annealed) — near-non-magnetic |
Selection rule for the 800 family: standard 800 covers general service and heat-treatment fixtures to about 600 °C; 800H (coarse grain + C 0.05–0.10 %) covers creep-controlled pressure service from about 600 °C; 800HT is specified when long design life above 700 °C — typically 760–900 °C reformer and cracker components — makes every extra MPa of rupture strength count. If your drawing says 800HT, the certificate must show N08811, C 0.06–0.10 %, Al+Ti 0.85–1.20 %, and a coarse-grain solution anneal.
| Industry | Typical 800HT components |
|---|---|
| Ethylene / petrochemical | Radiant and transfer-line tubing, quench-boiler internals in cracking furnaces |
| Hydrogen / reforming | Primary-reformer outlet manifolds, pigtails, headers — the classic 800HT duty |
| Gasification / syngas | Gasifier internals and high-temperature piping |
| Industrial heating | Electric heating-element sheaths, furnace tubes, radiant tubes, fixtures |
| Power & nuclear | High-temperature heat exchangers, steam superheaters |
| Chemical | Nitric-acid condensers and steam-heating coils where moderate corrosion plus heat coincide |
800HT welds readily with ERNiCr-3 (82) by GTAW/GMAW/SMAW, no preheat. Two heat-treatment disciplines matter. First, the mill solution anneal must be at least 1,149 °C with rapid cooling — this is what sets the coarse grain (ASTM No. 5 or coarser) that the creep data assume. Second, for weldments that will serve above about 538 °C, a stress-relief PWHT at about 899 °C (1 h per 25 mm of thickness, minimum 30 min) then air cooling is the standard precaution against relaxation cracking in service. Purchasing checks that actually protect you: (1) the certificate must state UNS N08811 — not N08810 — with the C and Al+Ti windows; (2) ask for the grain-size statement on the MTC; (3) hot forming runs in the 870–1,200 °C range followed by rapid cooling, and re-annealing after heavy cold deformation; (4) if the supplier cannot document the coarse-grain anneal, you are buying 800H metallurgy at 800HT prices.
We supply Incoloy 800HT seamless tube, plate, bar and — a core strength of ours — forged rings and machined-to-drawing parts for reformer and cracker service, with in-house ring rolling and machining. Every shipment goes out with EN 10204 3.1 mill certificates showing UNS, carbon and Al+Ti windows, and we verify PMI before packing. Typical lead time: 20 working days for forged rings and machined parts, quoted EXW Shanghai.
Same Fe-Ni-Cr base. 800HT narrows carbon to 0.06–0.10 %, forces Al+Ti into the 0.85–1.20 % window (800H only requires ≥ 0.30 %), and mandates a ≥ 1,149 °C coarse-grain solution anneal. Net effect: higher creep-rupture strength in long service above about 700 °C. PMI cannot tell them apart — audit the certificate.
Oxidation resistance extends to roughly 1,040–1,100 °C, and ASME design allowables for N08811 run to about 899 °C. The practical design zone for its creep advantage is roughly 650–900 °C; below about 600 °C, 800H or even standard 800 is usually sufficient and cheaper.
It is austenitic with low magnetic permeability (≈ 1.01 annealed) — effectively non-magnetic for most purposes, though a faint response is possible after heavy cold work.
For weldments serving above about 538 °C, yes — the standard precaution is a stress relief around 899 °C (1 h per 25 mm thickness, minimum 30 minutes) followed by air cooling, to avoid relaxation-related grain-boundary cracking in service.
Three items: the UNS number is N08811 (not N08810), carbon is 0.06–0.10 % with Al+Ti summing to 0.85–1.20 %, and the solution anneal temperature is stated at ≥ 1,149 °C with a grain-size note. If any of these is missing, you have no documented basis for calling the material 800HT.
Send us your drawing or specification for a quotation — we reply within one business day.